粘接塑料外壳 和模制件

例如,由透明塑料制成的护罩、保护板、艺术品、陈列柜、展示架、商店或展览货架和报架的塑料部件和模具通常只能通过粘接来连接。

塑料板通常采用边接或斜接。特殊的粘合剂还能使激光切割的边缘实现无应力裂缝粘合。而对于塑料板之间的大面积粘接,则需要使用非常柔软、有弹性的粘合剂。

许多此类粘合剂都具有高透明度,因此粘合后的接合处会与组件融为一体。边缘和斜面看起来就像由一整块木板拼接而成,再也看不出是粘合的接缝。

用透明塑料制成的宣传册架可以使用 Hoenle 粘合剂进行粘合。

下表列出了推荐用于粘接塑料外壳的部分 Hoenle 粘合剂。如需更多产品和定制解决方案,请联系我们。

要下载技术数据表 (TDS),请单击粘合剂名称。

用透明塑料制成的宣传册架可使用 Hoenle 粘合剂进行粘合

Adhesive Application Areas Viscosity [mPas] Base Curing Substrates Special Properties
- 1-3 cyanoacrylate moisture, room temperature
  • Ideal for bonding PVC, ABS, PA (Polyamid), PC, EPDM
  • Capillary flow
- 1-3 cyanoacrylate moisture, room temperature
  • Ideal for bonding PVC, ABS, PC, PA
  • Capillary flow
- 70-100 cyanoacrylate moisture, room temperature
  • Ideal for bonding PVC, ABS, PC, PA
  • Capillary flow
  • Bonding hose unions,
  • bridging large gaps,
  • suitable for porous materials
shear thinning cyanoacrylate moisture, room temperature
  • Ideal for bonding PA, PC, ABS, PVC, EPDM
  • Biocompatible: certified to USP Class VI standards
  • Plastic bonding,
  • metal bonding
30-50 cyanoacrylate moisture, room temperature
  • Ideal for bonding PVC, ABS, PA, PC, PMMA, aluminium, steel, copper
  • Instant adhesive
  • plastic bonder
  • perfect choice for mirror bonding
  • Bonding coloured plastics,
  • delicate bonds
230-350 (LVT, 25 °C, Sp. 2/60 rpm) cyanoacrylate moisture, room temperature
  • Ideal for bonding PVC, PMMA, ABS, PA, PC, EPDM, stainless steel
  • Film forming,
  • suitable for bonding porous materials,
  • biocompatible: certified to USP Class VI standards
- 4-12 (LVT, 25 °C, Sp. 2/60 rpm) cyanoacrylate moisture, room temperature
  • Ideal for bonding PMMA, PVC, ABS, PA (polyamid), PC (polycarbonate)
  • odorless
- 100,000-240,000 cyanoacrylate moisture, room temperature
  • Ideal for bonding polycarbonate (PC), PMMA, PVC, ABS, PA
  • Shear thinning
  • gel-like
- 7,000-15,000 mix (LVT, 25°C, Sp. 4/30 rpm) 2-part epoxy thermal, room temperature
  • Bonding thermoplastics and FR 4
  • High temperature resistance
  • short pot life
  • fast application
- 3,000-4,000 mix (LVT, 25°C, Sp. 4/30 rpm) 2-part epoxy thermal room temperature
  • Bonding glass, thermoplastics and FR 4
  • Very high adhesion to PC
  • resistant to moisture and chemicals
- 70-150 acrylate UV VIS
  • Bonding PC (Polycarbonate)
  • hard-PVC, PET, ABS, SAN
  • PMMA (Plexiglas®, acrylic glass)
  • Joining glass and plastics
  • Joining metals to plastics
  • Capillary flow
  • flexible and tear-proof adhesive
  • suitable for potting
  • dry surface
  • Bonding of flexible components;
  • Attaching components on PCBs
900-1,500 (LVT, 25°C, Sp. 3/30 rpm) acrylate UV VIS
  • Bonding PC /Makrolon, hard-PVC, PET, ABS, SAN, PMMA (Plexiglas®, acrylic glass)
  • Bonding glass, steel, stainless steel, aluminium, brass
  • Dry surface after curing,
  • biocompatible: certified to USP Class VI and ISO 10993-5 standards
  • Bonding of flexible components;
  • Attaching components on PCBs
4,000-8,000 acrylate UV VIS
  • bonding PC (Makrolon), hard-PVC, PET, ABS, SAN, PMMA (Plexiglas®, acrylic glass)
  • joining glass and plastics
  • joining metals to plastics
  • dry surface after curing
  • flexible and tear-proof
  • excellent adhesion to many plastics
- 7,000-9,000 acrylate UV VIS
  • Bonding PMMA (Plexiglas®, acrylic glass), hard-PVC, PET, ABS, SAN, PC
  • Joining glass and plastics
  • Joining metals to plastics
  • Very high adhesion to many plastics
  • dry surface after curing
  • flexible and tear-proof
- 700-1,000 acrylate UV VIS secondary heat cure
  • Bonding PC, PMMA (Plexiglas®, acrylic glass), hard-PVC, PET, ABS, SAN
  • Joining glass and plastics
  • Joining metals to plastics
  • Very high adhesion to many plastics
  • dry surface after curing
  • flexible and tear-proof
  • suitable for potting
  • Sealing electrical assemblies,
  • breathing masks
250-500 acrylate UV VIS
  • Bonding ABS, PMMA (Plexiglas®, acrylic glass), hard-PVC, PET, SAN, PC
  • Joining glass and plastics
  • Joining metals to plastics
  • Joining plastics with various substrates
  • Flexible,
  • well suited for bonding plastics with low UV translucence and permeable to visible light,
  • biocompatible: certified to USP Class VI standards
  • encapsulation of electronic components
  • CIPG and liquid seals
  • plastic bonding
  • plastic film lamination
  • medical technology
  • potting material
5,000-10,000 (Rheometer, 25°C, 10s^-1) acrylate UV VIS
  • Bonding PET, PMMA (Plexiglas®, acrylic glass), PC, ABS, SAN, hard-PVC
  • Joining plastics and glass
  • Joining plastics and metals
  • Joining plastics to various substrates
  • High resistance to thermal stress and moisture
  • Flexible and stable
  • Low shrinkage, optically clear
  • Joining dissimilar subjects
  • plastics /glass bonding
  • suitable for elastic bonding of large surfaces
30-100 acrylate UV VIS
  • Bonding PC (polycarbonate)
  • PVC, PMMA,
  • ABS, glass and metals
  • High resistance to alcohols and moisture
  • non-yellowing
  • very high adhesion to plastics, glass and metals
  • suitable for bonding large areas
  • certified according to USP Class VI
  • Bonding plastic parts
40-70 acrylate UV VIS
  • Bonding plastics such as
  • PC, PVC, ABS
  • Bonding glass and metals
  • Flexible
  • high elongation at break
  • perfect solution for bonding large surfaces
  • very high adhesion to plastics
  • glass and metals
- 100-300 acrylate UV VIS
  • Bonding PMMA (Plexiglas®, acrylic glass), PC, PVC
  • Very high shear strength and bond strength
  • excellent adhesion to plastics
  • capillary flow behavior
- 10-100 acrylate UV VIS
  • Bonding PMMA (Plexiglas®, acrylic glass), PC, PVC
  • Specially formulated for bonding PMMA
  • high adhesion
  • capillary flow
- 1,500-2,500 acrylate UV VIS
  • Bonding PMMA (Plexiglas®, acrylic glass), PC, PVC
  • Excellent adhesion to many plastics
  • high bond strength
  • excellent flow properties
  • Plastic bonding,
  • bonding containers
3,000-5,000 acrylate UV
  • Bonding hard-PVC, ABS, SAN, PUR, PC
  • Excellent adhesion to plastics, especially to PC and PMMA;
  • biocompatible: certified to USP Class VI standards
- 1,000-2,000 acrylate UV VIS
  • Bonding PMMA (Plexiglas®, acrylic glass), PC, PVC, ABS
  • Flexible
  • high resistance to moisture
  • cures thick layers of adhesive
- 15,000-25,000 acrylate UV VIS secondary heat cure
  • Bonding PMMA (Plexiglas®, acrylic glass), PC, PET, ABS, SAN, FR4, PBT, hard-PVC
  • Bonding plastics and metals
  • Acrylate-Hybrid
  • low thermal expansion
  • low shrinkage
  • impact resistant
  • dry surface
  • grey color
  • Potting
  • Sealing
  • Protection of sensitive components
19,000-32,000 (Rheometer, 25°C, 10s^-1) acrylate UV VIS
  • Bonding PMMA (Plexiglas®, acrylic glass), PC, PET, ABS, SAN, FR4, PBT, hard-PVC
  • Bonding plastics and metals
  • Acrylate hybrid
  • superior strength
  • low thermal expansion
  • impact resistant
  • low shrinkage
  • resistant to soldering stress
  • excellent flow properties
- 20,000-30,000 (Rheometer, 25°C, 50s^-1) acrylate UV VIS -
  • Acrylate hybrid
  • superior strength
  • low thermal expansion
  • low shrinkage
  • impact resistant
  • resistant to soldering stress
  • paste-like
  • stable and high viscous
- 12,000-30,000 acrylate UV VIS
  • Bonding PC (Polycarbonate), PMMA
  • Bonding plastics to glass
  • Elastic
  • high peel strength
  • optically clear
  • very flexible
  • stable gel
  • Encapsulation of electronic components
1,000-1,500 acrylate UV VIS
  • Bonding PC (Polycarbonate), PMMA
  • Bonding plastics to glass
  • Elastic
  • high peel strength
  • optically clear
  • very flexible
  • suitable for potting

*紫外线 = 320 – 390 纳米 可见光 = 405 纳米

联系方式 和支持